Key Takeaway
LBT/AXLE WELD CRACKS by L.B.T., INC. was recalled on July 3, 2001. What to do: LBT WILL REPLACE THE NEWAY AIR-RIDE SUSPENSION SYSTEM WITH A PRO-PAR FOUR-LEAF SPRING SUSPENSION AND WILL ALSO REPLACE THE TWO VEHICLE AXLES. OWNER N...
LBT/AXLE WELD CRACKS
Description
VEHICLE DESCRIPTION: FRUEHAUF LARGE CAPACITY PETROLEUM TRAILERS BUILT WITH TANDEM NEWAY AIR-RIDE SUSPENSION SYSTEMS. OPERATION OF THE TRAILERS HAS REVEALED A POSSIBILITY THAT THE AXLE BRACKET-TO-AXLE WELDS COULD CRACK, AND THE CRACKS COULD PROPAGATE INTO THE AXLE BEAM.
Injuries / Consequence
THE CRACKING COULD AFFECT VEHICLE STABILITY. THE REDUCTION IN VEHICLE STABILITY WOULD BE INDICATED TO THE OPERATOR BY ABNORMAL HANDLING CHARACTERISTICS SUCH AS SWAYING OF THE VEHICLE. IF THE OPERATOR DOES NOT HEED THE REDUCTION OF VEHICLE STABILITY, A VEHICLE CRASH COULD OCCUR IN THE FORM OF A ROLLOVER.
Remedy
LBT WILL REPLACE THE NEWAY AIR-RIDE SUSPENSION SYSTEM WITH A PRO-PAR FOUR-LEAF SPRING SUSPENSION AND WILL ALSO REPLACE THE TWO VEHICLE AXLES. OWNER NOTIFICATION IS EXPECTED TO BEGIN DURING JUNE/JULY 2001. OWNERS WHO TAKE THEIR VEHICLES TO AN AUTHORIZED DEALER ON AN AGREED UPON SERVICE DATE AND DO NOT RECEIVE THE FREE REMEDY WITHIN A REASONABLE TIME SHOULD CONTACT LBT AT 1-402-333-4900.
Products Affected
Vehicle
VehiclesRelated Recalls
Engine Stall Due to Disabled Rear Fuel Pump
March 5, 2026
Tire Sidewall Damage
March 5, 2026
Rearview Camera Image May Not Display
March 4, 2026
Incorrectly Displayed Rearview Camera Image/FMVSS 111
March 4, 2026
Driver's Seat May Move Unexpectedly
March 3, 2026
Driveshaft May Separate
March 3, 2026
Frequently Asked Questions
Is this recall still active?
Check the status badge at the top of this page. "Ongoing" means the recall is still active and you should follow the remedy instructions. "Completed" or "Terminated" means the recall process has concluded, though the safety issue remains relevant for any unrepaired products.
How do I check if my product is affected?
Compare the model number, lot code, serial number, or date range listed in the recall notice with the information on your product's label or packaging. For vehicles, check your VIN at NHTSA.gov/Recalls.
What remedy is available for this recall?
The listed remedy for this recall is: LBT WILL REPLACE THE NEWAY AIR-RIDE SUSPENSION SYSTEM WITH A PRO-PAR FOUR-LEAF SPRING SUSPENSION AND WILL ALSO REPLACE THE TWO VEHICLE AXLES. OWNER NOTIFICATION IS EXPECTED TO BEGIN DURING JUNE/JULY...
Where can I find the original recall notice?
This recall was issued by NHTSA. You can view the original notice using the link provided above.